Ottone

Ottone - UNI EN 1982:2017

LegaCuPbSnFeAlNiMnSbPSiZnSAsBiCdCrMgCoSe
CB750S
(1, 2)
min
max
63 1 - - - - - - - - 20 - - - - - - - -
66 2.8 1.5 0.7 0.1 1 0.2 - 0.02 0.04 40 - - - - - - - -
Ricerche correlate:
CC750S, CUZN33PB2-B, CUZN33PB2-C, SCB3, GB-CUZN33PB, GBCUZN33PB, GB-MS65A, GBMS65A
CB751S
(2)
min
max
63.5 0.8 - 0.25 - - - - - 0.7 20 - - - - - - - -
65.5 2 0.8 0.5 0.1 0.8 0.1 0.05 - 1 40 - - - - - - - -
Ricerche correlate:
CC751S, CUZN33PB2SI-B, CUZN33PB2SI-C
CB754S
(2, 15)
min
max
58 0.5 - - 0.1 - - - - - 20 - - - - - - - -
62 2.4 1 0.7 0.8 1 0.5 - 0.02 0.05 40 - - - - - - - -
Ricerche correlate:
CC754S, CUZN39PB1AL-B, CUZN39PB1AL-C, DCB3, CUZN40PB
CB766S
(2)
min
max
60 - - - 0.6 - - - - - 20 - - - - - - - -
63 0.4 0.4 0.4 1.8 1.8 0.4 0.05 0.02 0.5 40 - - - - - - - -
Ricerche correlate:
CC766S, CUZN37AL1-B, CUZN37AL1-C
CB767S
(2)
min
max
59 - - - 0.1 - - - - - 20 - - - - - - - -
64 0.1 0.1 0.4 0.8 0.8 0.4 - 0.05 0.05 40 - - - - - - - -
Ricerche correlate:
CC767S, CUZN38AL-B, CUZN38AL-C
CB770S
(3)
min
max
61.5 0.2 - - 0.5 - - - - - 30 - 0.04 - - - - - -
63.5 1.6 0.3 0.3 0.7 0.2 0.1 - - - 40 - 0.14 - - - - - -
CB773S
(3)
min
max
57 - - - 0.1 - - - - - 40 - - - - - - - -
59 0.1 0.3 0.3 0.3 0.02 0.02 0.02 0.02 0.02 50 - - - - - - - -
Ricerche correlate:
CC773S, CUZN42AL-B, CUZN42AL-C

Note

1 Per i lingotti utilizzati in colata in sabbia a tenuta di pressione e in colata in centrifuga, l'alluminio dev'essere 0.02% max
2 Nickel incluso nel conteggio del rame
3 Per applicazioni per acqua potabile, possono essere applicate alcune restrizioni alla composizione chimica di alcuni elementi in accordo con le regole/leggi nazionali
15 Per i lingotti utilizzati in colata in sabbia o in colata in centrifuga, l'alluminio dev'essere 0.02% max